Alloy Steel ASME SA335 Grade P5

Steel grade: ASTM A335 P5 Packing: Bare packing/bundle packing/crate packing/wooden protection at the both sides of tubes and suitably protected for sea-worthly delivery or as requested. Inspection and Test: Chemical Composition Inspection, Mechanical Properties Test(Tensile Strength,Yield Strength, Elongation, Flaring, Flattening, Bending, Hardness, Impact Test), Surface and Dimension Test,No-destructive Test, Hydrostatic Test. Surface treatment: Oil-dip, Varnish, Passivation,

Category:

Steel grade: ASTM A335 P5 Packing: Bare packing/bundle packing/crate packing/wooden protection at the both sides of tubes and suitably protected for sea-worthly delivery or as requested. Inspection and Test: Chemical Composition Inspection, Mechanical Properties Test(Tensile Strength,Yield Strength, Elongation, Flaring, Flattening, Bending, Hardness, Impact Test), Surface and Dimension Test,No-destructive Test, Hydrostatic Test. Surface treatment: Oil-dip, Varnish, Passivation,

Packing:

Bare packing/bundle packing/crate packing/wooden protection at the both sides of tubes and suitably protected for sea-worthily delivery or as requested.

Inspection and Test:

Chemical Composition Inspection, Mechanical Properties Test(Tensile Strength,Yield Strength, Elongation, Flaring, Flattening, Bending, Hardness, Impact Test), Surface and Dimension Test,No-destructive Test, Hydrostatic Test.

Surface treatment:

Oil-dip, Varnish, Passivation, Phosphating, Shot Blasting.
Both ends of each crate will indicate the order no., heat no., dimensions, weight and bundles or as requested.

ASTM A335 P5 Chemical Compositions(%)

Compositions Data
UNS Designa-tion K41545
Carbon(max.) 0.15
Manganese 0.30-0.60
Phosphorus(max.) 0.025
Silicon(max.) 0.50
Chromium 4.00-6.00
Molybdenum 0.45-0.65
Other Elements …
Mechanical properties for ASTM A335 P5

Properties Data
Tensile strength, min, (MPa) 415 Mpa
Yield strength, min, (MPa) 205 Mpa
Elongation, min, (%), L/T 30/20
Material & Manufacture

Pipe may be either hot finished or cold drawn with the finishing heat treatment noted below.

Heat Treatment

– A / N+T

– N+T / Q+T

– N+T

Mechanical Tests Specified

– Transverse or Longitudinal Tension Test and Flattening Test, Hardness Test, or Bend Test

– For material heat treated in a batch-type furnace, tests shall be made on 5% of the pipe from each treated lot. For small lots, at least one pipe shall be tested.

– For material heat treated by the continuous process, tests shall be made on a sufficient number of pipe to constitute 5% of the lot, but in no case less than 2 pipe.